Please use this identifier to cite or link to this item:
doi:10.22028/D291-24624
Title: | Enhancement of fracture strength of cutted plate glass by the application of SiO2 sol-gel coatings |
Author(s): | Endres, Klaus Mennig, Martin Amlung, Martin Gier, Andreas Schmidt, Helmut K. |
Language: | English |
Year of Publication: | 1999 |
OPUS Source: | High-performance coatings for transparent systems in large-area and, or high-volume applications : September 6 - 10, 1998 / 2nd International Conference on Coatings on Glass, ICCG. [H. Pulker ..., ed.]. - Amsterdam : Elsevier, 1999, S. 204-208 |
SWD key words: | Glasscheibe Glas Biegefestigkeit Sol-Gel-Verfahren Rasterelektronenmikroskop Tetraethylsilicat <Tetraethylorthosilicat> |
DDC notations: | 620 Engineering and machine engineering |
Publikation type: | Conference Paper |
Abstract: | The influence of SiO2 sol-gel coatings on the bending strength of soda lime plate glass samples has been investigated by 3 point bending and double ring bending strength measurements. The samples were prepared by manual glass cutting and were coated with two different types of SiO2 coating: A TEOS coating (thickness of about 100 nm) was obtained from sols synthesized by acid catalysis of tetraethoxysilane and a MTKS coating (thickness of about 1 µm) was obtained from a methyl modified nanoparticulate SiO2 sol. The coatings were applied by dipping and were densified at 500'°C for 1 h. The fracture strength σ0 of edge coated plate glass (60 X 25 X 3.8 mm), determined by 3 point bending test (according to EN 843-1), was increased after coating with TEOS from σ0 = 24 MPa to 40 MPa (67% increase). The fracture strength increased to σ0 = 56 MPa (133% increase) on applying MTKS or a double coating of TEOS followed by MTKS. The evaluation of these measurements using Weibull statistical analysis resulted in m values of 4.1 and 4.2 for the TEOS and MTKS coating and 3.5 for double coating (uncoated glasses m = 5.7), respectively. These results combined with high resolution secondary electron microscopy investigations led to the conclusion that the strengthening effect of the two different sol-gel systems is due to a partial flaw healing and clamping of the crack sides. |
Link to this record: | urn:nbn:de:bsz:291-scidok-29328 hdl:20.500.11880/24680 http://dx.doi.org/10.22028/D291-24624 |
ISBN: | 0-444-50247-5 |
Date of registration: | 9-Jul-2010 |
Faculty: | SE - Sonstige Einrichtungen |
Department: | SE - INM Leibniz-Institut für Neue Materialien |
Collections: | INM SciDok - Der Wissenschaftsserver der Universität des Saarlandes |
Files for this record:
File | Description | Size | Format | |
---|---|---|---|---|
sm199915.pdf | 2,48 MB | Adobe PDF | View/Open |
Items in SciDok are protected by copyright, with all rights reserved, unless otherwise indicated.