Title: | Pt/SiO2. - Part IV: Isotopic exchange between cyclopentane and deuterium |
Author(s): | Inoue, Yasunobu Burwell, Robert L. Butt, John B. Cohen, Jerome B. Herrmann, Jean M. Schmidt, Helmut K. |
Language: | English |
Year of Publication: | 1978 |
OPUS Source: | Journal of catalysis. - 53. 1978, 3, S. 401-413 |
SWD key words: | Cyclopentanderivate Deuterium Helium Wasserstoff |
DDC notations: | 620 Engineering and machine engineering |
Publikation type: | Journal Article |
Abstract: | Isotopic exchange between cyclopentane and deuterium, mostly at 81°C, has been investigated on a set of 10 Pt/SiO2 catalysts whose percentages exposed ranged from 6.3 to 81%. The standard pretreatment, O2, 300°C; H2, 300°C; He 450°C with cooling in helium, leads to turnover numbers for formation of exchanged cyclopentanes, which decline by a factor of less than 2 as the percentage exposed increases from 6.3 to 63.5% and then at 81% rise to about the value for 6.3%. Selectivity to various exchanged species varies with percentage exposed and, in particular, D6/D10 (the ratio of initial yields of d6 and d10) decreases substantially as the percentage exposed increases. This suggests that exchange of the hydrogen atoms on both sides of the cyclopentane ring proceeds mainly via formation of α,α-diadsorbed cyclopentane on catalysts with a smaller percentage exposed and by rollover on catalysts with a large percentage exposed. Other pretreatment conditions such as O2, 300 °C; H2, 100 °C and O2, 300 °C; H2, 450 °C with cooling in hydrogen give larger structure sensitivities for activity and different selectivities. Catalysts deactivate rather rapidly but with little change in selectivity. Deactivation is accompanied by the formation of carbonaceous residues. C/Pts becomes approximately 0.5 and the activity declines 10% in about 10 min on stream. Ninety percent or more of the carbon in the residue occurs in a cyclopentane structure because 90% of the carbon is removed as cyclopentane by hydrogen at 100 °C. Repetition of the standard pretreatment regenerates the initial activity and selectivity. |
Link to this record: | urn:nbn:de:bsz:291-scidok-25731 hdl:20.500.11880/24344 http://dx.doi.org/10.22028/D291-24288 |
Date of registration: | 23-Dec-2009 |
Faculty: | SE - Sonstige Einrichtungen |
Department: | SE - INM Leibniz-Institut für Neue Materialien |
Collections: | INM SciDok - Der Wissenschaftsserver der Universität des Saarlandes |
Files for this record:
File | Description | Size | Format | |
---|---|---|---|---|
sm197801.pdf | 2 MB | Adobe PDF | View/Open |
Items in SciDok are protected by copyright, with all rights reserved, unless otherwise indicated.