Bitte benutzen Sie diese Referenz, um auf diese Ressource zu verweisen:
doi:10.22028/D291-24547
Titel: | Development of electrochromic smart windows by sol-gel techniques |
VerfasserIn: | Munro, Brian Krämer, Stefanie Zapp, Patrick Krug, Herbert Schmidt, Helmut K. |
Sprache: | Englisch |
Erscheinungsjahr: | 1997 |
Quelle: | Sol-gel optics IV : 30 July-1 August 1997, San Diego, California / Bruce S. Dunn ... [et al.], chairs/editors. - Bellingham, Wash. : SPIE, c1997. - (SPIE proceedings series ; 3136), S. 470-479 |
Kontrollierte Schlagwörter: | Sol-Gel-Verfahren Elektrochromie Lithiumion Nanokomposit Elektrolyt |
DDC-Sachgruppe: | 620 Ingenieurwissenschaften und Maschinenbau |
Dokumenttyp: | Konferenzbeitrag (in einem Konferenzband / InProceedings erschienener Beitrag) |
Abstract: | A novel nanocomposite lithium ion-conducting electrolyte has been developed, based on organically modified silanes, which is suitable for application in a sol-gel electrochromic system. The system developed consists of FTO-coated (Fluorine doped Tin Oxide) glass coated with tungsten oxide, WO3, at one side of the device as the electrochromic layer, with a cerium oxide-titanium oxide layer, CeO2-TiO2, acting as ion-storage layer or counter electrode. The adhesive properties of the electrolyte enabled the manufacture of electrochromic devices in a laminated structure: glassFTOWO3 anocomp.elect.CeO2-TiO2FTOglass. The conductivity of the nanocomposite electrolyte system varies between 10-4 and 10-5 Scm-1 at 25°C depending on the exact composition. The temperature dependence of the conductivity exhibits typical Vogel-Tamman-Fulcher (VTF) behaviour. The thickness of the electrolyte between the two halves of the device could be adjusted by the use of a spacer technique in the range 10 - 150 µm. Optoelectrochemical measurements were conducted on electrochromic devices to study the kinetics of colouration and bleaching as a function of the number of switching cycles. At present, cells are constructed in two formats:10 X 15 cm2 and 35 X 35 cm2. Switching times under one minute were achieved for the smaller format with a corresponding optical modulation between 75% to 20% (at λ = 0.633 µm). In the case of the larger format the switching time increases to several minutes due to the increase in geometric area. |
Link zu diesem Datensatz: | urn:nbn:de:bsz:291-scidok-28513 hdl:20.500.11880/24603 http://dx.doi.org/10.22028/D291-24547 |
ISBN: | 0-8194-2558-3 |
Datum des Eintrags: | 6-Mai-2010 |
Fakultät: | SE - Sonstige Einrichtungen |
Fachrichtung: | SE - INM Leibniz-Institut für Neue Materialien |
Sammlung: | INM SciDok - Der Wissenschaftsserver der Universität des Saarlandes |
Dateien zu diesem Datensatz:
Datei | Beschreibung | Größe | Format | |
---|---|---|---|---|
sm199722.pdf | 1,29 MB | Adobe PDF | Öffnen/Anzeigen |