Titel: Coloration mechanisms of sol-gel NiO-TiO2 layers studied by EQCM
VerfasserIn: Al-Kahlout, Amal
Aegerter, Michel A.
Sprache: Englisch
Erscheinungsjahr: 2007
Quelle: Solar energy materials & solar cells. - 91. 2007, 4, S. 213-223
Kontrollierte Schlagwörter: Sol-Gel-Verfahren
Elektrochromie
Elektrolyt
DDC-Sachgruppe: 620 Ingenieurwissenschaften und Maschinenbau
Dokumenttyp: Journalartikel / Zeitschriftenartikel
Abstract: An electrochemical quartz crystal microbalance was used as a sensitive detector to analyse the mass changes occurring during the coloration/bleaching processes of sol—gel NiO—TiO2 electrochromic layers. Double layers were deposited on gold-coated quartz crystal electrode and sintered at 300 °C in air. The electrochemical process was studied in KOH electrolyte in the potential range -0.4 to +0.57 V vs. SCE during 650 CV cycles. The current density, charge and mass were found to increase with cycling. The shape of the mass spectrum is rather complex and changes continuously by cycling. The mass of the layer increases after each cycle slowly up to about the 150th cycle then it increases strongly after about the 250th cycle. It passes through a maximum around the 570th cycle with high amplitude variation within each cycle and then decreases fast without drastic change of the cathodic charge. Finally, a complete breakdown occurs around the 650th CV cycle impeding to record any further mass variation. The study is divided in two typical regions where the mechanism of coloration is found to change by cycling. During the first 150 CV cycles, the reversible change of the mass with the charge (increase in the anodic range for V>0.35 V vs. SCE and decrease in the cathodic range for V<-0.2 V) was related to exchange of OH- groups that involves a change of the oxidation state of Ni from 2+ to 3+ and vice versa leading to coloration and bleaching processes, respectively. For further cycling a model is proposed taking into account the incorporation of K(H2O)n+ ions in the hydrated structure of the layer. The irreversible increase of both the mass and charge exchanged during each cycle is interpreted as due to an increase of the amount of Ni(OH)2.
Link zu diesem Datensatz: urn:nbn:de:bsz:291-scidok-25594
hdl:20.500.11880/24272
http://dx.doi.org/10.22028/D291-24216
Datum des Eintrags: 17-Nov-2009
Fakultät: SE - Sonstige Einrichtungen
Fachrichtung: SE - INM Leibniz-Institut für Neue Materialien
Sammlung:INM
SciDok - Der Wissenschaftsserver der Universität des Saarlandes

Dateien zu diesem Datensatz:
Datei Beschreibung GrößeFormat 
inm200701.pdf596,33 kBAdobe PDFÖffnen/Anzeigen


Alle Ressourcen in diesem Repository sind urheberrechtlich geschützt.